Material Notes:
Polyethylene 18BOA is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easily on automatic molding equipment to produce molded items with excellent gloss, clarity, and warpage resistance. This formula complies with FDA regulations at 21 CFR177.1520 (c)(2.2) for use in articles for packing and holding food during cooking. Users must make their own determination that their use of this product is safe, legal, and technically suitable for their intended applications.Unless otherwise noted, all tests are run at 23°C and 50% RH.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D4883
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 8.00 MPa
1160 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Tensile Strength, Yield 11.0 MPa
1600 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Elongation at Break 90 %
90 %
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Flexural Modulus 0.228 GPa
33.1 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C
194 °F
ASTM D1525
Brittleness Temperature -45.0 °C
-49.0 °F
ASTM D746
Descriptive Properties Value Comments
Process Injection Molding