Material Notes:
7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.86 g/cc
0.320 lb/in³
Annealed
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 621 - 724 MPa
90000 - 105000 psi
Tensile Strength, Yield >= 517 MPa
>= 75000 psi
0.2% offset
Elongation at Break >= 6.0 %
>= 6.0 %
in 2 in.
Tensile Modulus 131 GPa
19000 ksi
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 300 °C
10.0 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 15.6 W/m-K
108 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 97 %
97 %
Nickel, Ni 2.0 %
2.0 %
Silicon, Si 0.40 %
0.40 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000445 ohm-cm
0.00000445 ohm-cm
Annealed