Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® XE 4188 nat PA612

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® XE 4188 nat PA612.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilamid XE 4188 natural is a high viscosity, unreinforced, impact resistant polyamide 612 (PA612) extrusion grade. Unique features of Grilamid XE 4188 natural are: High viscosityImpact resistantGood chemical and zinc-chloride resistanceGood hydrolysis resistanceLow water absorptionHeat and UV resistantEasy processing Application examples: Grilamid XE 4188 natural has been developed for rigid automotive and industrial tubing such as found in fuel, coolant fluid, oil or hydraulic systems.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Water Absorption 2.7 %
2.7 %
ISO 62
Moisture Absorption 1.20 %
1.20 %
ISO 62
Linear Mold Shrinkage, Flow 0.030 cm/cm
0.030 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
0.0040 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 70.0 MPa
10200 psi
conditioned; ISO 2039-1
100 MPa
14500 psi
dry; ISO 2039-1
Tensile Strength, Yield 45.0 MPa
6530 psi
dry; ISO 527-1/-2
50.0 MPa
7250 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
<= 50 %
<= 50 %
dry; ISO 527-1/-2
Elongation at Yield 5.0 %
5.0 %
dry; ISO 527-1/-2
20 %
20 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.30 GPa
189 ksi
conditioned; ISO 527-1/-2
1.80 GPa
261 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 5.00 J/cm²
23.8 ft-lb/in²
dry; ISO 179/1eA
9.00 J/cm²
42.8 ft-lb/in²
conditioned; ISO 179/1eA
1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 160 µm/m-°C
88.9 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
Melting Point 218 °C
424 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
dry; IEC 60093
1.00e+10 ohm-cm
1.00e+10 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Strength 38.0 kV/mm
965 kV/in
dry; IEC 60243-1
38.0 kV/mm
965 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Air intake sytems
Compressed air systems
Fuel systems
Hydraulic systems
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Processing Other Extrusion
Product Attributes High viscosity
Hydrolysis resistant
Improved alcohol resistance
Special Characteristics High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)
Users viewing this material also viewed the following: