Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® XE 3997 nat PAMACM12

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® XE 3997 nat PAMACM12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilamid XE 3997 natural is a transparent thermoplastic polyamide based on aliphatic and cycloaliphatic blocks. Grilamid XE 3997 natural is particularly suitable for blow molded bottles and offers a variety of interesting properties such as: High transparencyLight and clear natural colorToughnessStiffnessFDA approvedLow densityComfortable surface feelSuitable for IBM & ISBM processes Grilamid XE 3997 natural can be used as an alternative to bisphenol A (BPA) containing materials, as well as for the production of optical and technical demanding parts in application fields such as: Baby careHousewarePackagingBlow-molded containersInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Water Absorption 3.0 %
3.0 %
ISO 62
Moisture Absorption 1.50 %
1.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 90.0 MPa
13100 psi
conditioned; ISO 2039-1
Tensile Strength at Break 45.0 MPa
6530 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 60.0 MPa
8700 psi
conditioned; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 6.0 %
6.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.60 GPa
232 ksi
conditioned; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
conditioned; ISO 179/1eA
1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Maximum Service Temperature, Air 80.0 - 100 °C
176 - 212 °F
long term; EMS
120 °C
248 °F
short term; EMS
Transformation Temperature, Tg 155 °C
311 °F
10°C/min; ISO 11357-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 34.0 kV/mm
864 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Food contact EU Requirements
FDA
Form Granules
Medical FDA
Packaging Blow moulded containers
Injectionstretchblowmoulded containers
Processing Extrusion - blow molding
Injection (stretch) blow molding
Other Extrusion
Special Characteristics Transparent
Users viewing this material also viewed the following: