EMS-Grivory Grivory® XE 3841 nat PA12

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® XE 3841 nat PA12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilamid XE 3841 is a flexible, heat stabilized and plasticizer-free Polyamide 12, which offers a very good processability for extrusion. Grilamid XE 3841 is qualified in Europe for direct contact with foodstuffs and alcoholic beverages. The main features of Grilamid XE 3841 are: Plasticizer freeVery flexibleTranslucentGood low temperature impact strengthLow density Grilamid XE 3841 is suitable for use on Tubes used in the food preparation industry as well as pneumatic tubes.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
ISO 1183
Water Absorption 1.1 %
1.1 %
ISO 62
Moisture Absorption 0.600 %
0.600 %
ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
conditioned, 15s; ISO 868
Tensile Strength at Break 30.0 MPa
4350 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 20.0 MPa
2900 psi
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 15 %
15 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.350 GPa
50.8 ksi
conditioned; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched NB
NB
conditioned; ISO 179/1eA
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 160 µm/m-°C
88.9 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 100 °C
176 - 212 °F
long term; EMS
130 °C
266 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 45.0 °C
113 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C
104 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 43.0 kV/mm
1090 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 575 V
575 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Food contact EU Requirements
FDA
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Processing Other Extrusion
Product Attributes Flexible
Special Characteristics High impact or impact modified