EMS-Grivory Grivory® TSS/2 FA PA666

Category Polymer , Thermoplastic , Nylon , Nylon 6/66
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® TSS/2 FA PA666.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon TSS/2 FA is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/2 FA has the following important properties: Excellent flow behaviorHigh toughnessVery good surface finishEasy processing Grilon TSS is used typically for various applications in the automotive, the electro and the sports & leisure field such as loudspeaker grids, interior casings, chair rollers, handles and levers. According to FDA (21 CFR 177.1500 and corresponding paragraphs covering the additives) GRILON TSS/2 FA is also approved for the direct contact with non-alcoholic foodstuffs.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption 8.0 %
8.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.012 cm/cm
0.012 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 80.0 MPa
11600 psi
conditioned; ISO 2039-1
140 MPa
20300 psi
dry; ISO 2039-1
Tensile Strength, Yield 55.0 MPa
7980 psi
conditioned; ISO 527-1/-2
80.0 MPa
11600 psi
dry; ISO 527-1/-2
Elongation at Break 5.0 %
5.0 %
dry; ISO 527-1/-2
5.0 %
5.0 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 4.0 %
4.0 %
dry; ISO 527-1/-2
15 %
15 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.40 GPa
203 ksi
conditioned; ISO 527-1/-2
3.30 GPa
479 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
dry; ISO 179/1eU
10.0 J/cm²
47.6 ft-lb/in²
conditioned; ISO 179/1eU
6.00 J/cm²

@Temperature 30.0 °C
28.6 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
8.00 J/cm²

@Temperature 30.0 °C
38.1 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
dry; ISO 179/1eA
1.00 J/cm²
4.76 ft-lb/in²
conditioned; ISO 179/1eA
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 70.0 - 100 °C
158 - 212 °F
long term; EMS
200 °C
392 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 25.0 kV/mm
635 kV/in
conditioned; IEC 60243-1
27.0 kV/mm
686 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
dry; IEC 60112
600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Food contact EU Requirements
FDA
Form Granules
Industry & Consumer goods Housewares
Sports & Leisure
Packaging Medical packaging
Processing Injection Molding