Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® TR XE 4010 PA*-I

Category Polymer , Thermoplastic , Nylon
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® TR XE 4010 PA*-I.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilamid XE 4010 is an amorphous cycloaliphatic copolyamide based on 58 % renewable resources. The material is designed for applications where high chemical resistance, high fatigue strength and toughness is required. The material is resistant to boiling water, a broad range of chemicals and to stress cracking. Articles can be easily produced by injection molding or extrusion. Grilamid XE 4010 offers a variety of interesting properties such as: High transparencyHigh glossHigh fatigue strengthResistance to boiling waterResistance to a broad range of solvents and chemicalsExcellent toughnessLow densityOutstanding weather resistance Grilamid XE 4010 is suitable for optical and technically demanding parts.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ISO 1183
Water Absorption 3.8 %
3.8 %
ISO 62
Moisture Absorption 1.80 %
1.80 %
ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 110 MPa
16000 psi
conditioned; ISO 2039-1
Tensile Strength at Break 55.0 MPa
7980 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 65.0 MPa
9430 psi
conditioned; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 7.0 %
7.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.70 GPa
247 ksi
conditioned; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
conditioned; ISO 179/1eA
1.00 J/cm²

@Temperature 30.0 °C
4.76 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
Maximum Service Temperature, Air 60.0 - 80.0 °C
140 - 176 °F
long term; EMS
90.0 °C
194 °F
short term; EMS
Transformation Temperature, Tg 118 °C
244 °F
10°C/min; ISO 11357-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75-1/-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 40.0 kV/mm
1020 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Additives Lubricants
Automotive Compressed air systems
Fuel systems
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Energy distribution
Lighting
Mobile phones and other portable devices
Form Granules
Industry & Consumer goods Housewares
Mechanical Engineering
Medical devices
Optics Spectacle frames
Processing Injection Molding
Product Attributes Bio based Polyamide
Co Polyamide
Hydrolysis resistant
Transparent Polyamide
Special Characteristics High impact or impact modified