Material Notes:
Product description: Grilamid TR 90 TL is a transparent thermoplastic polyamide based on aliphatic, cycloaliphatic and aromatic blocks. The special characteristic of Grilamid TR 90 TL is the high stiffness combined with excellent chemical resistance and high transparency. Key features are: Increased stiffnessHigh transparency and glossHigh flexural fatigue strengthHigh chemical and stress crack resistanceGood impact strengthLow density Grilamid TR 90 TL is especially suitable for stable injection moulding applications requiring high flow and good de-moulding properties. Typical application fields are: Spectacle framesMechanical engineeringSanitary applicationsDomestic appliancesAutomotive interiorElectro / ElectronicsInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ISO 1183
Water Absorption 2.5 %
2.5 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 120 MPa
17400 psi
conditioned; ISO 2039-1
Tensile Strength at Break 55.0 MPa
7980 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 75.0 MPa
10900 psi
conditioned; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 7.0 %
7.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.85 GPa
268 ksi
conditioned; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
conditioned; ISO 179/1eA
1.10 J/cm²

@Temperature 30.0 °C
5.23 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 95.0 µm/m-°C
52.8 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 95.0 µm/m-°C
52.8 µin/in-°F
ISO 11359-1/-2
Maximum Service Temperature, Air 80.0 - 100 °C
176 - 212 °F
long term; EMS
110 °C
230 °F
short term; EMS
Transformation Temperature, Tg 135 °C
275 °F
10°C/min; ISO 11357-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 33.0 kV/mm
838 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Additives Lubricants
Automotive Compressed air systems
Exterior
Fuel systems
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Energy distribution
Lighting
Mobile phones and other portable devices
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Medical devices
Processing Injection Molding
Product Attributes Co Polyamide
Hydrolysis resistant
Transparent Polyamide
Special Characteristics High impact or impact modified