Material Notes:
Product description: Grilamid TR 55 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 55 natural offers outstanding properties such as:TransparencyUnlimited colorabilityStress crack resistanceToughness and stiffnessGood chemical resistanceEU and FDA food approval Grilamid TR 55 natural is especially suited for injection molded applications in the application fields of: OpticsAutomotiveMechanical engineeringSafety technologyElectro / ElectronicsSanitaryDomestic appliancesSport & LeisureInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Water Absorption 3.5 %
3.5 %
ISO 62
Moisture Absorption 1.50 %
1.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 120 MPa
17400 psi
conditioned; ISO 2039-1
Tensile Strength, Yield 75.0 MPa
10900 psi
conditioned; ISO 527-1/-2
75.0 MPa
10900 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
<= 50 %
<= 50 %
dry; ISO 527-1/-2
Elongation at Yield 7.0 %
7.0 %
dry; ISO 527-1/-2
9.0 %
9.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 2.20 GPa
319 ksi
conditioned; ISO 527-1/-2
2.20 GPa
319 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
dry; ISO 179/1eA
0.800 J/cm²
3.81 ft-lb/in²
conditioned; ISO 179/1eA
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Maximum Service Temperature, Air 80.0 - 100 °C
176 - 212 °F
long term; EMS
120 °C
248 °F
short term; EMS
Transformation Temperature, Tg 160 °C
320 °F
10°C/min; ISO 11357-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 31.0 kV/mm
787 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Cooling and climate control
Fuel systems
Interior
Powertrain and Chassis
Electricals & Electronics Cables & Tubes
Electrical appliances
Electrical equipment
Energy distribution
Lighting
Mobile phones and other portable devices
Food contact EU Requirements
FDA
Form Granules
Industry & Consumer goods Heating systems
Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Medical devices
Power transmission
Sanitary, water and gas supply
Sports & Leisure
Tools & Accessories
Medical FDA
USP VI
Optics Lenses
Optical components
Packaging Cosmetics / Personal care
Medical packaging
Non oriented film
Processing Injection Molding
Other Extrusion
Special Characteristics Transparent
Water Contact DVGW W270
KTW
NSF 61
WRAS