Material Notes:
Product description: Grilamid LV-3 ESD is an antistatic PA12 injection molding grade, with fiber reinforcement of 30%. Due to its special formulation, the material can be used for applications where electrostatic discharge behavior and good fuel resistance is required. Application examples: Connectors for fuel systems with antistatic properties.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ISO 1183
Water Absorption 1.1 %
1.1 %
ISO 62
Moisture Absorption 0.600 %
0.600 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 81
81
conditioned, 15s; ISO 868
83
83
dry, 15s; ISO 868
Tensile Strength at Break 110 MPa
16000 psi
conditioned; ISO 527-1/-2
125 MPa
18100 psi
dry; ISO 527-1/-2
Elongation at Break 5.0 %
5.0 %
dry; ISO 527-1/-2
7.0 %
7.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 7.00 GPa
1020 ksi
conditioned; ISO 527-1/-2
7.80 GPa
1130 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
conditioned; ISO 179/1eU
8.50 J/cm²
40.4 ft-lb/in²
dry; ISO 179/1eU
6.50 J/cm²

@Temperature 30.0 °C
30.9 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
7.00 J/cm²

@Temperature 30.0 °C
33.3 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
dry; ISO 179/1eA
1.50 J/cm²
7.14 ft-lb/in²
conditioned; ISO 179/1eA
1.00 J/cm²

@Temperature 30.0 °C
4.76 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.00 J/cm²

@Temperature 30.0 °C
4.76 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
27.8 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C
194 - 248 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 90.0 °C
194 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
dry; IEC 60093
1.00e+6 ohm-cm
1.00e+6 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+6 ohm
1.00e+6 ohm
IEC 60093
Descriptive Properties Value Comments
Automotive Fuel systems
Form Granules
Processing Injection Molding
Product Attributes Hydrolysis resistant
Special Characteristics Anti-static
High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)