EMS-Grivory Grivory® LV-2H PA12-GF20

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, 20% Glass Fiber Filled
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® LV-2H PA12-GF20.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilamid LV-2H is a 20% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensional stabilityvery high elongation at breakgood chemical resistancegood UV Stabilityhigh impact strength Grilamid LV-2H is suitable for production of technical parts in the application fields of: Electrical & electronic componentsAutomotiveSafety componentsMechanical engineeringDomestic appliancesAnalytical and medical devicesSports & leisure goodsInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 1183
Water Absorption 1.2 %
1.2 %
ISO 62
Moisture Absorption 0.600 %
0.600 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
conditioned, 15s; ISO 868
Tensile Strength at Break 90.0 MPa
13100 psi
conditioned; ISO 527-1/-2
105 MPa
15200 psi
dry; ISO 527-1/-2
Elongation at Break 7.0 %
7.0 %
dry; ISO 527-1/-2
10 %
10 %
conditioned; ISO 527-1/-2
Tensile Modulus 4.40 GPa
638 ksi
conditioned; ISO 527-1/-2
5.50 GPa
798 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
conditioned; ISO 179/1eU
8.00 J/cm²
38.1 ft-lb/in²
dry; ISO 179/1eU
7.50 J/cm²

@Temperature 30.0 °C
35.7 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
conditioned; ISO 179/1eA
1.50 J/cm²

@Temperature 30.0 °C
7.14 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
16.7 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 150 µm/m-°C
83.3 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C
194 - 248 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 150 °C
302 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 80.0 °C
176 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 35.0 kV/mm
889 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Air intake sytems
Automotive electr. and electronics, lighting
Compressed air systems
Cooling and climate control
Fuel systems
Hydraulic systems
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Mobile phones and other portable devices
Form Granules
Industry & Consumer goods Heating systems
Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Medical devices
Power transmission
Sanitary, water and gas supply
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Hydrolysis resistant
Special Characteristics High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)