Material Notes:
Product description: Grilamid LV-23 ESD is a 20% fiber reinforced, anti-static injection molding grade Polyamide 12 (PA12). Grilamid LV-23 ESD is heat stabilized, is easy to process and demold. The inherent color of this product is black. The main features of Grilamid LV-23 ESD are: Electrically conductive/ anti-staticHeat stabilizedHigh stiffness and strengthGood chemical resistanceGood oil resistanceHigh surface qualityGood dimensional stabilityLow density, low weight Grilamid LV-23 ESD is suitable for the production of injection molded parts in the area of electro/electronics and in the automotive industry for anti-static housings, covers and small components.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Water Absorption 1.0 %
1.0 %
ISO 62
Moisture Absorption 0.500 %
0.500 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
conditioned, 15s; ISO 868
Tensile Strength at Break 95.0 MPa
13800 psi
conditioned; ISO 527-1/-2
110 MPa
16000 psi
dry; ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
dry; ISO 527-1/-2
5.0 %
5.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 5.00 GPa
725 ksi
conditioned; ISO 527-1/-2
5.80 GPa
841 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
conditioned; ISO 179/1eU
4.00 J/cm²

@Temperature 30.0 °C
19.0 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
conditioned; ISO 179/1eA
0.600 J/cm²

@Temperature 30.0 °C
2.86 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 150 µm/m-°C
83.3 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C
194 - 248 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 150 °C
302 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 80.0 °C
176 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
conditioned; IEC 60093
Surface Resistance 10000 ohm
10000 ohm
IEC 60093
Descriptive Properties Value Comments
Automotive Fuel systems
Form Granules
Processing Injection Molding
Product Attributes Hydrolysis resistant
Special Characteristics Anti-static
High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)