Material Notes:
Product Description: Grilamid L 25 Z is a UV- and heat stabilized high viscosity polyamide 12 grade with improved toughness. A special feature of Grilamid L25 Z is its high energy absorption capacity Application examples: Grilamid L 25 Z has been designed for protecting aerial cables from shotgun damage. Due to its outstanding toughness, the integration of a layer of Grilamid L 25 Z in an aerial cable improves its shotgun protection and allows reduction of other costly armoring.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Water Absorption 1.5 %
1.5 %
ISO 62
Moisture Absorption 0.700 %
0.700 %
ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cm
0.0080 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
conditioned, 15s; ISO 868
Ball Indentation Hardness 55.0 MPa
7980 psi
conditioned; ISO 2039-1
Tensile Strength at Break 40.0 MPa
5800 psi
dry; ISO 527-1/-2
40.0 MPa
5800 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 35.0 MPa
5080 psi
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
>= 50 %
>= 50 %
dry; ISO 527-1/-2
Elongation at Yield 12 %
12 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.900 GPa
131 ksi
conditioned; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 5.50 J/cm²
26.2 ft-lb/in²
conditioned; ISO 179/1eA
1.30 J/cm²

@Temperature 30.0 °C
6.19 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 140 µm/m-°C
77.8 µin/in-°F
ISO 11359-1/-2
Melting Point 179 °C
354 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
140 °C
284 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C
104 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 22.0 kV/mm
559 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Compressed air systems
Fuel systems
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Processing Other Extrusion
Product Attributes High viscosity
Special Characteristics High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)