Material Notes:
Product Description: Grilamid L 20 G grey 9280 is a medium viscosity, unreinforced, heat stabilized polyamide 12 for injection molding and cable sheathing. The main features of this product are: Low moisture absorptionHigh dimensional stabilityExcellent wear and abrasion resistanceLow friction coefficientGood heat resistanceExcellent chemical resistanceLow density Grilamid L20 G grey 9280 is suitable for technical parts in the application fields of: Automotive Mechanical engineeringDomestic appliancesInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ISO 1183
Water Absorption 1.5 %
1.5 %
ISO 62
Moisture Absorption 0.700 %
0.700 %
ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cm
0.0080 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
conditioned, 15s; ISO 868
Tensile Strength at Break 50.0 MPa
7250 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 40.0 MPa
5800 psi
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 12 %
12 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.10 GPa
160 ksi
conditioned; ISO 527-1/-2
Charpy Impact Unnotched 10.0 J/cm²
47.6 ft-lb/in²
conditioned; ISO 179/1eU
10.0 J/cm²

@Temperature 30.0 °C
47.6 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
conditioned; ISO 179/1eA
0.600 J/cm²

@Temperature 30.0 °C
2.86 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 140 µm/m-°C
77.8 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 100 °C
194 - 212 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Powertrain and Chassis
Electricals & Electronics Cables & Tubes
Connectors
Form Granules
Industry & Consumer goods Housewares
Mechanical Engineering
Medical devices
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Other Extrusion
Product Attributes Improved friction & wear properties
Special Characteristics High impact or impact modified
Improved heat resistance