EMS-Grivory Grivory® HT2V-3X V0 nat 6059 PA6T/66-GF30

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 30% Glass Fiber Reinforced
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® HT2V-3X V0 nat 6059 PA6T/66-GF30.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT2V-3X V0 is halogen free and free of red phosphorous. RoHS: Grivory HT2V-3X V0 is in compliance with RoHS (2002/95/EC, Restriction of Hazardous Substances) WEEE: Parts produced from Grivory HT2V-3X V0 are not subject to "selective treatment" according the Directive 2002/96/EC on Waste Electrical and Electronic Equipment. ISO polymer designation: PA 6T/66 ASTM-designation: PPA, polyphthalamide. The main distinguishing feature of Grivory HT, when compared to other polyamides, is its good performance at high temperatures providing parts which are stiffer, stronger and have better heat distortion stability and chemical resistance. Grivory HT2V-3X V0 is especially suitable for injection molded parts in electrical and electronic applications with high requirements and a material flame class acc. UL 94 V-0. The Material is suitable for lead-free SMT reflow soldering acc. e.g. JEDEC J-STD-020C (peak temperature 260°C). Components conforming to JEDEC MSL2 are achievable.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ISO 1183
Water Absorption 3.5 %
3.5 %
ISO 62
Moisture Absorption 1.30 %
1.30 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 230 MPa
33400 psi
conditioned; ISO 2039-1
240 MPa
34800 psi
dry; ISO 2039-1
Tensile Strength at Break 130 MPa
18900 psi
conditioned; ISO 527-1/-2
140 MPa
20300 psi
dry; ISO 527-1/-2
Elongation at Break 2.0 %
2.0 %
dry; ISO 527-1/-2
2.0 %
2.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 10.5 GPa
1520 ksi
conditioned; ISO 527-1/-2
10.5 GPa
1520 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
dry; ISO 179/1eU
4.00 J/cm²
19.0 ft-lb/in²
conditioned; ISO 179/1eU
3.50 J/cm²

@Temperature 30.0 °C
16.7 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
3.50 J/cm²

@Temperature 30.0 °C
16.7 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
dry; ISO 179/1eA
0.700 J/cm²
3.33 ft-lb/in²
conditioned; ISO 179/1eA
0.600 J/cm²

@Temperature 30.0 °C
2.86 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.600 J/cm²

@Temperature 30.0 °C
2.86 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 45.0 µm/m-°C
25.0 µin/in-°F
ISO 11359-1/-2
Melting Point 310 °C
590 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 150 °C
302 °F
long term; EMS
240 °C
464 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 280 °C
536 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 190 °C
374 °F
ISO 75-1/-2
Flammability, UL94 V-0
V-0
IEC 60695-11-10
5VA
5VA
IEC 60695-11-20
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
IEC 60695-11-10
Oxygen Index 35 %
35 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
dry; IEC 60093
1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 34.0 kV/mm
864 kV/in
dry; IEC 60243-1
34.0 kV/mm
864 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Interior
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Energy distribution
Lighting
Mobile phones and other portable devices
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Mechanical Engineering
Power transmission
Tools & Accessories
Processing Injection Molding
Product Attributes Co Polyamide
Improved alcohol resistance
Improved flowability and demoulding
Partially aromatic Polyamide
Special Characteristics Flame retardant
Improved heat resistance