Material Notes:
Product description: Grivory XE 4027 natural is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewable raw materials. Grivory XE 4027 natural is free of halo-gens and red phosphorus. RoHS: Grivory XE 4027 natural is in compliance with RoHS (2002/95/EC, Restriction of Hazardous Substances). WEEE: Parts produced from Grivory XE 4027 natural are not subject to "selective treatment" according the Directive 2002/96/EC on Waste Electrical and Electronic Equipment. ISO polymer designation: PA 10T/X ASTM designation: PPA, polyphthalamide. The main distinguishing features of Grivory HT, when compared to other poly-amides, are its good performance at high temperatures providing parts which are stiffer, stronger, have better heat distortion and dimensional stability as well as excellent chemical resistance and low moisture absorption. Grivory XE 4027 natural is especially suitable for injection molded components in electrical and electronic applications which require a flame class acc. UL 94 V-0. The material is suitable for lead-free SMT reflow soldering acc. e.g. JEDEC J-STD-020C (peak temperature 260°C). Components conforming to JEDEC MSL1 are achievable.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Water Absorption 2.3 %
2.3 %
ISO 62
Moisture Absorption 0.900 %
0.900 %
ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 235 MPa
34100 psi
dry; ISO 2039-1
235 MPa
34100 psi
conditioned; ISO 2039-1
Tensile Strength at Break 130 MPa
18900 psi
dry; ISO 527-1/-2
130 MPa
18900 psi
conditioned; ISO 527-1/-2
Elongation at Break 2.0 %
2.0 %
dry; ISO 527-1/-2
2.0 %
2.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 10.0 GPa
1450 ksi
conditioned; ISO 527-1/-2
10.0 GPa
1450 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
dry; ISO 179/1eU
5.00 J/cm²
23.8 ft-lb/in²
conditioned; ISO 179/1eU
5.00 J/cm²

@Temperature 30.0 °C
23.8 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
5.00 J/cm²

@Temperature 30.0 °C
23.8 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
dry; ISO 179/1eA
0.800 J/cm²
3.81 ft-lb/in²
conditioned; ISO 179/1eA
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
38.9 µin/in-°F
ISO 11359-1/-2
Melting Point 295 °C
563 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 150 °C
302 °F
long term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 155 °C
311 °F
ISO 75-1/-2
Flammability, UL94 V-0
V-0
IEC 60695-11-10
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
dry; IEC 60093
1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 33.0 kV/mm
838 kV/in
dry; IEC 60243-1
33.0 kV/mm
838 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Exterior
Fuel systems
Interior
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Energy distribution
Lighting
Mobile phones and other portable devices
Form Granules
Processing Injection Molding
Product Attributes Bio based Polyamide
Hydrolysis resistant
Special Characteristics Flame retardant
Improved heat resistance
Improved UV resistance (outdoor use)