Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® F 34 NL PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® F 34 NL PA6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grilon F 34 NL nat. 6019 is a medium viscosity PA 6 containing nucleation and lubrication suitable for the production of coex blown films and mono or coex cast films. Grilon F 34 NL nat. 6019 has been developed for flexible film applications.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption 9.0 %
9.0 %
ISO 62
Moisture Absorption 2.50 %
2.50 %
ISO 62
Water Vapor Transmission 20.0 g/m²/day
1.29 g/100 in²/day
23°C/85%r.h.; DIS 15106-1/-2
Oxygen Transmission Rate 25.0 cc/m²/day
1.61 cc/100 in²/day
23°C/0%r.h.; DIS 15105-1/-2
70.0 cc/m²/day
4.51 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
Carbon Dioxide Transmission 80.0 cc-mm/m²-24hr-atm
203 cc-mil/100 in²-24hr-atm
23°C/0%r.h.; DIS 15105-1/-2
250 cc-mm/m²-24hr-atm
635 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
Melt Flow 40 g/10 min
40 g/10 min
(MVR) [cm³/10min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Modulus 0.750 GPa
109 ksi
conditioned; ISO 527-1/-2
3.00 GPa
435 ksi
dry; ISO 527-1/-2
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3
Optical Properties Metric English Comments
Gloss 100 %
100 %
60°; ISO 2813
Descriptive Properties Value Comments
Food contact EU Requirements
FDA
Form Granules
Gelboflextest [holes/m²], EMS 700
Packaging Non oriented film
Oriented film
Paper coating
Tubes
Processing Blown Film Extrusion
Film Extrusion
Other Extrusion
Product Attributes Barrier Properties
High viscosity
Nucleated
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved