EMS-Grivory Grivory® CA 6 E PA*

Category Polymer , Thermoplastic , Nylon
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® CA 6 E PA*.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon CA 6 E is a non-extracted copolyamide with a low melting point. Grilon CA 6 E characterizes itself through the following properties Very high flexibility and toughnessVery good thermoforming and orientation propertiesHigh shrinkVery good transparencyLow melting point (130°C) Grilon CA 6E is suitable for use as a middle layer of a multi layer structure. Suitable applications include flexible packaging for foodstuffs such as shrinkable film for consumer packaging E.g meat, cheese, sausage and fish.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Water Absorption 5.0 %
5.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Water Vapor Transmission 20.0 g/m²/day
1.29 g/100 in²/day
23°C/85%r.h.; DIS 15106-1/-2
Oxygen Transmission Rate 150 cc/m²/day
9.66 cc/100 in²/day
23°C/0%r.h.; DIS 15105-1/-2
250 cc/m²/day
16.1 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
Carbon Dioxide Transmission 450 cc-mm/m²-24hr-atm
1140 cc-mil/100 in²-24hr-atm
23°C/0%r.h.; DIS 15105-1/-2
850 cc-mm/m²-24hr-atm
2160 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
Melt Flow 250 g/10 min
250 g/10 min
(MVR) [cm³/10min]; ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 20.0 MPa
2900 psi
ISO 527-3
Film Tensile Strength at Yield, TD 18.0 MPa
2610 psi
ISO 527-3
Film Elongation at Break, MD 900 %
900 %
ISO 527-3
Film Elongation at Break, TD 900 %
900 %
ISO 527-3
Film Elongation at Yield, MD 15 %
15 %
ISO 527-3
Film Elongation at Yield, TD 15 %
15 %
ISO 527-3
Tensile Modulus 0.350 GPa
50.8 ksi
conditioned; ISO 527-1/-2
Tear Strength 65.0 kN/m
371 pli
Trouser Tear resistance MD; ISO 6383-1
65.0 kN/m
371 pli
Trouser Tear resistance TD; ISO 6383-1
Elmendorf Tear Strength MD 8160 g
8160 g
ISO 6383-2
Elmendorf Tear Strength TD 8160 g
8160 g
ISO 6383-2
Film Tensile Strength at Break, MD 90.0 MPa
13100 psi
ISO 527-3
Film Tensile Strength at Break, TD 60.0 MPa
8700 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 130 °C
266 °F
10°C/min; ISO 11357-1/-3
Optical Properties Metric English Comments
Gloss 130 %
130 %
60°; ISO 2813
Descriptive Properties Value Comments
Food contact EU Requirements
Form Granules
Gelboflextest [holes/m²], EMS 100
Packaging Oriented film
Processing Blown Film Extrusion
Film Extrusion
Other Extrusion
Product Attributes Barrier Properties
Co Polyamide
Flexible
High viscosity
Special Characteristics Transparent