EMS-Grivory Grivory® BG-40 S PA6-GF40

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® BG-40 S PA6-GF40.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon BG-40 S is a normal viscosity PA 6 injection molding type with 40% glass fibers. Grilon BG-40 S has the following important properties: High stiffnessExcellent surface finishEasy flowingEasy processingApplication examples are stressed functional parts for automotive applications and housings for electro power tools.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183
Water Absorption 7.0 %
7.0 %
ISO 62
Moisture Absorption 1.50 %
1.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 150 MPa
21800 psi
conditioned; ISO 527-1/-2
230 MPa
33400 psi
dry; ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
dry; ISO 527-1/-2
5.0 %
5.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 8.50 GPa
1230 ksi
conditioned; ISO 527-1/-2
11.6 GPa
1680 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
dry; ISO 179/1eU
8.00 J/cm²
38.1 ft-lb/in²
conditioned; ISO 179/1eU
7.00 J/cm²

@Temperature 30.0 °C
33.3 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
7.50 J/cm²

@Temperature 30.0 °C
35.7 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
dry; ISO 179/1eA
2.00 J/cm²
9.52 ft-lb/in²
conditioned; ISO 179/1eA
0.900 J/cm²

@Temperature 30.0 °C
4.28 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C
194 - 248 °F
long term; EMS
160 °C
320 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 165 °C
329 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 35.0 kV/mm
889 kV/in
conditioned; IEC 60243-1
37.0 kV/mm
940 kV/in
dry; IEC 60243-1
Comparative Tracking Index 550 V
550 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Interior
Electricals & Electronics Electrical appliances
Electrical equipment
Form Granules
Processing Injection Molding