Material Notes:
Product description: Grilon BG-30 FC is a heat stabilised PA6 injection moulding grade with 30% glass fibres. Grilon BG-30 FC has the following important properties: High stiffnessExcellent surface finishShort cycle timesEasy flowingEasy processing Application examples are stressed functional parts with a difficult wall thickness to flowlength ratio, such as housings for electro/electronic machines or automotive air ducts or other functional parts in the engine compartment.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Water Absorption 7.0 %
7.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 110 MPa
16000 psi
conditioned; ISO 2039-1
230 MPa
33400 psi
dry; ISO 2039-1
Tensile Strength at Break 100 MPa
14500 psi
conditioned; ISO 527-1/-2
180 MPa
26100 psi
dry; ISO 527-1/-2
Elongation at Break 2.5 %
2.5 %
dry; ISO 527-1/-2
7.0 %
7.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 6.20 GPa
899 ksi
conditioned; ISO 527-1/-2
10.0 GPa
1450 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
dry; ISO 179/1eU
8.00 J/cm²
38.1 ft-lb/in²
conditioned; ISO 179/1eU
5.50 J/cm²

@Temperature 30.0 °C
26.2 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
5.50 J/cm²

@Temperature 30.0 °C
26.2 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
dry; ISO 179/1eA
1.50 J/cm²
7.14 ft-lb/in²
conditioned; ISO 179/1eA
0.900 J/cm²

@Temperature 30.0 °C
4.28 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.900 J/cm²

@Temperature 30.0 °C
4.28 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 110 - 130 °C
230 - 266 °F
long term; EMS
200 °C
392 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 37.0 kV/mm
940 kV/in
conditioned; IEC 60243-1
40.0 kV/mm
1020 kV/in
dry; IEC 60243-1
Comparative Tracking Index 500 V
500 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Air intake sytems
Interior
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Form Granules
Industry & Consumer goods Housewares
Mechanical Engineering
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Improved flowability and demoulding
Copyright © lookpolymers.com All Rights Reserved