EMS-Grivory Grivory® BFZ 3 PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® BFZ 3 PA6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon BFZ 3 is an unreinforced, high impact resistant PA6 extrusion grade. Grilon BFZ 3 has the following important properties: Extreme toughnessEasy processingLow density Grilon BFZ 3 is used in coextrusion as a barrier layer and to improve the mechanical properties of blow molded parts.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Water Absorption 9.0 %
9.0 %
ISO 62
Moisture Absorption 3.00 %
3.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.011 cm/cm
0.011 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 40.0 MPa
5800 psi
conditioned; ISO 2039-1
95.0 MPa
13800 psi
dry; ISO 2039-1
Tensile Strength, Yield 25.0 MPa
3630 psi
dry; ISO 527-1/-2
50.0 MPa
7250 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
<= 50 %
<= 50 %
dry; ISO 527-1/-2
Elongation at Yield 4.0 %
4.0 %
dry; ISO 527-1/-2
15 %
15 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.600 GPa
87.0 ksi
conditioned; ISO 527-1/-2
1.80 GPa
261 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 6.50 J/cm²
30.9 ft-lb/in²
dry; ISO 179/1eA
11.5 J/cm²
54.7 ft-lb/in²
conditioned; ISO 179/1eA
1.50 J/cm²

@Temperature 30.0 °C
7.14 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.50 J/cm²

@Temperature 30.0 °C
7.14 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 130 µm/m-°C
72.2 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 150 µm/m-°C
83.3 µin/in-°F
ISO 11359-1/-2
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
160 °C
320 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 39.0 kV/mm
991 kV/in
conditioned; IEC 60243-1
42.0 kV/mm
1070 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Electricals & Electronics Cables & Tubes
Food contact EU Requirements
FDA
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Mechanical Engineering
Power transmission
Tools & Accessories
Packaging Blow moulded containers
Injectionstretchblowmoulded containers
Processing Extrusion - blow molding
Injection Molding
Other Extrusion
Product Attributes Barrier Properties
Flexible
Special Characteristics High impact or impact modified
Users viewing this material also viewed the following: