EMS-Grivory Grivory® 1S XE 4224 nat PA1010

Category Polymer , Thermoplastic , Nylon
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® 1S XE 4224 nat PA1010.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Grilamid XE 4224 natural is a heat and UV stabilized high viscosity polyamide 1010 (PA1010), designed for extrusion. In addition the product can be used for thicker injection molded articles. Grilamid XE 4224 is characterized by the following product profile: Close to 100% based on renewable resourcesGood chemical and UV resistanceDuctile, resilientLow moisture absorptionHigh dimensional stabilityLow density Grilamid XE 4224 natural is suitable for applications in areas like: Consumer goods Automotive functional parts Semi-fabricates Tubes, film, sheet, profilesCable sheathing and protectionInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Water Absorption 2.1 %
2.1 %
ISO 62
Moisture Absorption 1.00 %
1.00 %
ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 80.0 MPa
11600 psi
conditioned; ISO 2039-1
110 MPa
16000 psi
dry; ISO 2039-1
Tensile Strength, Yield 50.0 MPa
7250 psi
conditioned; ISO 527-1/-2
55.0 MPa
7980 psi
dry; ISO 527-1/-2
Elongation at Break 30 %
30 %
dry; ISO 527-1/-2
45 %
45 %
conditioned; ISO 527-1/-2
Elongation at Yield 5.0 %
5.0 %
dry; ISO 527-1/-2
20 %
20 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.30 GPa
189 ksi
conditioned; ISO 527-1/-2
2.00 GPa
290 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
dry; ISO 179/1eA
0.900 J/cm²
4.28 ft-lb/in²
conditioned; ISO 179/1eA
0.600 J/cm²

@Temperature 30.0 °C
2.86 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
dry; IEC 60093
1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Strength 38.0 kV/mm
965 kV/in
dry; IEC 60243-1
38.0 kV/mm
965 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Powertrain and Chassis
Electricals & Electronics Cables & Tubes
Connectors
Form Granules
Industry & Consumer goods Housewares
Mechanical Engineering
Sports & Leisure
Tools & Accessories
Processing Film Extrusion
Other Extrusion
Product Attributes Bio based Polyamide
High viscosity
Nucleated
Special Characteristics Improved heat resistance
Improved UV resistance (outdoor use)