EMS-Griltech Grilamid® HP 1200 Nylon 12 Fiber (Staple Length = 51)

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer EMS-Griltech
Trade Name Grilamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Griltech Grilamid® HP 1200 Nylon 12 Fiber (Staple Length = 51).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: GRILAMID HP 1200 is a Nylon 12 fiber used in hybrid yarns and as a matrix in composite materials.Data provided by EMS-Griltech.
Physical Properties Metric English Comments
Fiber Count 3.30 dtex
2.97 denier
Descriptive Properties Value Comments
Color Raw White
Luster Bright
Staple Length 48-54 mm