ELASTO UK Dryflex® 3005-101 TPE, Modified Injection Molding Grade for Vacuum Cleaner Seals

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer ELASTO UK Ltd, a Hexpol company
Trade Name Dryflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ELASTO UK Dryflex® 3005-101 TPE, Modified Injection Molding Grade for Vacuum Cleaner Seals.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3005-101 is specifically designed for vacuum cleaner seals.Information from Vita Thermoplastic Polymers (VTP).Vita Thermoplastic Polymers was aquired by HEXPOL and is now ELASTO
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ISO 2781
Melt Flow 20 g/10 min

@Load 5.00 kg,
Temperature 230 °C
20 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 25
25
ISO 868
Tensile Strength at Break 3.00 MPa
435 psi
ISO 37
Elongation at Break 850 %
850 %
ISO 37
100% Modulus 0.000500 GPa
0.0725 ksi
ISO 37
Tear Strength 10.0 kN/m
57.1 pli
Method C; ISO 34
Descriptive Properties Value Comments
Color Black