Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 93
93
ASTM D2240
Tensile Strength, Ultimate 48.98 MPa
7104 psi
ASTM D412
Elongation at Break 369 %
369 %
ASTM D412