E-Polymers Tekaster® F615G45 , 45% Glass Fiber Reinforced PET

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 50% Glass Reinforced
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKASTER®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers Tekaster® F615G45 , 45% Glass Fiber Reinforced PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
45% Glass Fiber reinforced, High strength, Information provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.69 g/cc
0.0611 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 195 MPa
28300 psi
ASTM D638
Elongation at Break 2.1 %
2.1 %
ASTM D638
Flexural Yield Strength 300 MPa
43500 psi
ASTM D790
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D790
Izod Impact, Notched 1.15 J/cm
2.15 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Processing Temperature 270 - 300 °C
518 - 572 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F