Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKALOY®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers Tekaloy® T80FR , Flame Retardant Un-Reinforced PBT/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame RetardantInformation provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength, Yield 33.0 MPa
4790 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Yield Strength 54.0 MPa
7830 psi
ASTM D790
Flexural Modulus 1.70 GPa
247 ksi
ASTM D790
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
ASTM D648
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F