Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

E-Polymers Tekaloy® G70A3 , Heat Resistance, Easy Molding PC/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKALOY®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers Tekaloy® G70A3 , Heat Resistance, Easy Molding PC/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat Resistance, Easy MoldingInformation provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Melt Flow 6.5 g/10 min

@Load 2.16 kg,
Temperature 250 °C
6.5 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 114
114
ASTM D785
Tensile Strength, Yield 59.0 MPa
8560 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Flexural Yield Strength 80.0 MPa
11600 psi
ASTM D790
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Izod Impact, Notched 6.50 J/cm
12.2 ft-lb/in
ASTM D256
4.50 J/cm

@Temperature -30.0 °C
8.43 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Processing Temperature 220 - 290 °C
428 - 554 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Users viewing this material also viewed the following: