Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

E-Polymers TEKAPPO® JF201 Filler Reinforced Heat Resistant Dimensional Stability Flame Retardant M-PPO

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKAPPO®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers TEKAPPO® JF201 Filler Reinforced Heat Resistant Dimensional Stability Flame Retardant M-PPO.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance and reinforced fiberglass. It shows high dimensional stability and rigidity used for housing and electrical parts.Information Provided by E-Polymers Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
Linear Mold Shrinkage, Transverse 0.0030 cm/cm
0.0030 in/in
Mechanical Properties Metric English Comments
Tensile Strength 124.6 MPa
18070 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 156.96 MPa
22765 psi
ASTM D790
Flexural Modulus 10.5 GPa
1520 ksi
ASTM D790
Izod Impact, Notched 0.510 J/cm
0.955 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 129 °C
264 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 123 °C
253 °F
ASTM D648
Flammability, UL94 V-1
V-1
Processing Properties Metric English Comments
Melt Temperature 280 - 310 °C
536 - 590 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F