Material Notes:
Precise injection, high crystallinityInformation provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 1.7 %
1.7 %
23°C/24 hr; ASTM D570
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D786
Tensile Strength, Yield 77.0 MPa
11200 psi
ASTM D638
Elongation at Break 80 %
80 %
ASTM D638
Flexural Yield Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 2.70 GPa
392 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.20 mm
NB

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 220 °C
428 °F
ASTM D2133
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
347 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Arc Resistance 195 sec
195 sec
Tungsten electrode; ASTM D495
Processing Properties Metric English Comments
Processing Temperature 230 - 250 °C
446 - 482 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F