Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

E-Polymers TEKAMID® TB120G30 , 30% Glass Fiber Reinforced PA6, DAM

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKAMID®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers TEKAMID® TB120G30 , 30% Glass Fiber Reinforced PA6, DAM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass Fiber Reinforced, Good impact resistanceInformation provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
Water Absorption 1.1 %
1.1 %
23°C/24 hr; ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 170 MPa
24700 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 230 MPa
33400 psi
ASTM D790
Flexural Modulus 7.90 GPa
1150 ksi
ASTM D790
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D2133
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Processing Temperature 270 - 290 °C
518 - 554 °F
Mold Temperature 80.0 - 90.0 °C
176 - 194 °F