E-Polymers TEKAMID® TA210M40 , 40% Mineral Filled PA66, DAM

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Mineral Filled
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKAMID®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers TEKAMID® TA210M40 , 40% Mineral Filled PA66, DAM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ASTM D792
Water Absorption 0.60 %
0.60 %
23°C/24 hr; ASTM D570
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM D786
Tensile Strength, Yield 95.0 MPa
13800 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Flexural Yield Strength 143 MPa
20700 psi
ASTM D790
Flexural Modulus 7.20 GPa
1040 ksi
ASTM D790
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 30.0 - 40.0 µm/m-°C

@Temperature 20.0 °C
16.7 - 22.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 260 °C
500 °F
ASTM D2133
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Processing Temperature 280 - 300 °C
536 - 572 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F