Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

E-Polymers TEKAMID® TA210HS , Heat Stabilized PA66, DAM

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Heat Stabilized
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKAMID®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers TEKAMID® TA210HS , Heat Stabilized PA66, DAM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat stabilizedInformation provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 1.3 %
1.3 %
23°C/24 hr; ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D786
Tensile Strength, Yield 83.0 MPa
12000 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Yield Strength 120 MPa
17400 psi
ASTM D790
Flexural Modulus 3.00 GPa
435 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.260 W/m-K
1.80 BTU-in/hr-ft²-°F
Melting Point 260 °C
500 °F
ASTM D2133
Deflection Temperature at 0.46 MPa (66 psi) 230 °C
446 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ASTM D648
Flammability, UL94 V-2
V-2
Electrical Properties Metric English Comments
Arc Resistance 185 sec
185 sec
Tungsten electrode; ASTM D495
Processing Properties Metric English Comments
Processing Temperature 270 - 290 °C
518 - 554 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F