Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend , Nylon
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKAMID®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers TEKAMID® H12TW Unreinforced Low warpage PA/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/ABS alloy (Unreinforced, GF reinforced, MR reinforced)Information Provided by E-Polymers Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Water Absorption 1.0 %

@Time 86400 sec
1.0 %

@Time 24.0 hour
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
Mechanical Properties Metric English Comments
Tensile Strength 63.765 MPa
9248.3 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Strength 107.91 MPa
15651 psi
ASTM D790
Flexural Modulus 2.5506 GPa
369.93 ksi
ASTM D790
Izod Impact, Notched 0.588 J/cm
1.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Melt Temperature 220 °C
428 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F