Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

E-Polymers TEKALOY® G75NHT Brominated Flame Retardant High Impact PC/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKALOY®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers TEKALOY® G75NHT Brominated Flame Retardant High Impact PC/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability. PC/PBT is usually used for automotive applications with good resistance against oils and solvents as well as high impact. PC/PET has an excellent surface and its high heat resistance allows it to be employed in housing for electrical appliances.Information Provided by E-Polymers Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Mechanical Properties Metric English Comments
Tensile Strength 58.86 MPa
8537 psi
ASTM D638
Elongation at Break >= 50 %
>= 50 %
ASTM D638
Flexural Strength 83.39 MPa
12090 psi
ASTM D790
Flexural Modulus 2.2563 GPa
327.25 ksi
ASTM D790
Izod Impact, Notched 6.86 J/cm
12.9 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
ASTM D648
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Melt Temperature 220 - 260 °C
428 - 500 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F