Dynasol Solprene® 375 Solution Random SBR

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Dynasol
Trade Name Solprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dynasol Solprene® 375 Solution Random SBR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Solprene 375 is a tin coupled, random styrene-butadiene copolymer with 24% styrene content. It is extended with naphtenic oil. S-375 is used as ingredient in compounds for battery cases, tires, cables, vulcanized shoe soles and industrial rubber goods. It can replace SBR 1778 types. The bales are wrapped in low melting point polyethylene film.Information provided by Dynasol.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
DIN 53479
Mooney Viscosity 46

@Temperature 100 °C
46

@Temperature 212 °F
ML 1+4; ASTM D1646
<= 80

@Temperature 100 °C
<= 80

@Temperature 212 °F
Compounded, ML 1+4; ASTM D1646
Ash <= 0.20 %
<= 0.20 %
ASTM D1416
Collected Volatile Condensable Material <= 0.75 %
<= 0.75 %
ASTM D1416
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 12.6 MPa
>= 1830 psi
Compounded, 35 mins.; ASTM D3185
Elongation at Break >= 450 %
>= 450 %
Compounded; ASTM D3185
300% Modulus 0.00950 GPa
1.38 ksi
Compounded, 35 mins.; ASTM D3185
Descriptive Properties Value Comments
Antioxidant Content 0.4 %
NM 300-52
Free Soap Max 0.03 %
ASTM D1416
Naphthenic Oil 37.5 phr
NM 300-42
Organic Acid Max 0.03 %
ASTM D1416
Styrene Content 24 %
NM 202-27