Dynasol Solprene® 233 Medium CIS Polybutadiene

Category Polymer , Thermoset
Manufacturer Dynasol
Trade Name Solprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dynasol Solprene® 233 Medium CIS Polybutadiene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Solprene 233 is a medium cis polybutadiene used in applications where good performance at low temperatures and excellent abrasion resistance are needed. It is designed for critical processing applications with enhanced mixing and processability. It is packaged in bales wrapped with low melting point polyethylene film.Information provided by Dynasol.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
DIN 53479
Mooney Viscosity 35

@Temperature 100 °C
35

@Temperature 212 °F
ML 1+4; ASTM D1646
<= 75

@Temperature 100 °C
<= 75

@Temperature 212 °F
Compounded, ML 1+4; ASTM D1646
Ash <= 0.25 %
<= 0.25 %
ASTM D1416
Collected Volatile Condensable Material <= 1.0 %
<= 1.0 %
ASTM D1416
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 11.0 MPa
>= 1600 psi
Compounded, 35 mins.; ASTM D3185
Elongation at Break >= 360 %
>= 360 %
Compounded; ASTM D3185
300% Modulus 0.00800 GPa
1.16 ksi
Compounded, 35 mins.; ASTM D3185
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -92.0 °C
-134 °F
NM 300-58
Descriptive Properties Value Comments
Antioxidant Content 0.2 %
NM 300-52
Color Max 3
NM 300-39
Free Soap Max 0.03 %
ASTM D1416
Organic Acid Max 0.03 %
ASTM D1416