Dynasol Calprene® H6110 Hydrogenated Rubber SEBS

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Dynasol
Trade Name Calprene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dynasol Calprene® H6110 Hydrogenated Rubber SEBS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Calprene H 6110 is a 70/30 Ethylene-Butylene/Styrene thermoplastic copolymer, polymerized in solution and having a linear structure with excellent ozone resistance.This product is available in:CH 6110 - porous pelletCH6110 P - powder form dusted WITH amorphous silicaCH 6110 PH - powder form WITHOUT any dusting agentApplications:Adhesives/sealantsOil gelsPlastic modificationBitumen modificationInformation provided by Dynasol
Physical Properties Metric English Comments
Volatiles <= 0.50 %
<= 0.50 %
ASTM D-5668
Brookfield Viscosity 470 cP

@Temperature 25.0 °C
470 cP

@Temperature 77.0 °F
0.2; MA 04-3-064
Viscosity Measure 6.0 cSt
6.0 cSt
Toluene solution viscosity 5,23%; MA 04-3-003
Melt Flow 1.5 g/10 min

@Load 16.0 kg,
Temperature 230 °C
1.5 g/10 min

@Load 35.3 lb,
Temperature 446 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
ASTM D-2240
Chemical Properties Metric English Comments
Styrene Content 30 %
30 %
on polymer; MA 04-3-062
Descriptive Properties Value Comments
Hunterlab color, max 3
Saturation, % min 99