Dynasol Calprene® 401 Thermoplastic Rubber SBS Dry

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Dynasol
Trade Name Calprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dynasol Calprene® 401 Thermoplastic Rubber SBS Dry.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Calprene 401 is an 80/20 Butadiene/Styrene thermoplastic copolymer, polymerized in solution and having a radial structure. This product is presented in porous crumb form.Applications:Bitumen modificationFootwearMechanical rubber goodsPlastic modificationInformation provided by Dynasol
Physical Properties Metric English Comments
Volatiles <= 0.50 %
<= 0.50 %
ASTM D-5668
Brookfield Viscosity 9700 cP
9700 cP
25% toluene solution; MA 04-3-064
Viscosity Measure 20 cSt
20 cSt
Toluene solution viscosity 5,23%; MA 04-3-003
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ASTM D-2240
Chemical Properties Metric English Comments
Styrene Content 20 %
20 %
on polymer; ASTM D-5775
Descriptive Properties Value Comments
Anti-sticking agent (calcium stearate), % 0.2
Hunterlab color, max 2
Insolubles in toluene, 325 mesh, % max 0.1