Material Notes:
DYMAX® Magnet Bonder™ Adhesives for Higher Performance and Lower CostDymax 535-A Magnet Bonder™ ActivatorEnvironmentally safe; no ODC's; alcohol carrier assures thin film. Typical Use: For use with Magnet Bonder™ 2000, 2010, 2020 adhesives
Descriptive Properties Value Comments
Color Amber to Brown
Viscosity Liquid