Dymax Magnet Bonder™ 2020 Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Dymax Corporation
Trade Name Magnet Bonder™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dymax Magnet Bonder™ 2020 Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DYMAX® Magnet Bonder™ Adhesives for Higher Performance and Lower CostDymax 2020 Magnet Bonder™ AdhesiveAcrylic and methacrylic acid-free; bond ferrite to metal, plated metals, E-coat, sealed cans Typical Use: D.C. motor magnet to can bonding
Mechanical Properties Metric English Comments
Shear Strength 20.7 MPa
3000 psi
Processing Properties Metric English Comments
Cure Time 0.500 - 0.667 min
0.00833 - 0.0111 hour
Fixture Rate
Descriptive Properties Value Comments
Color Translucent
Gap Fill 0.02 in.
Viscosity Gel