Dymax 9-984-B Conformal Coating

Category Polymer , Adhesive , Thermoset
Manufacturer Dymax Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dymax 9-984-B Conformal Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9-984-B Conformal CoatingCures to an opaque black finish; hides components or circuitry from view; protects sensitive circuits from light. Cure Speed (fpm): 2 - 6 Cure Type: UV, Visible and Heat
Physical Properties Metric English Comments
Viscosity 6000 cP
6000 cP
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 41.4 MPa
6000 psi
Descriptive Properties Value Comments
Cure Depth 0.07 in.