Dymax 9-20558 Conformal Coating

Category Polymer , Adhesive , Thermoset
Manufacturer Dymax Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dymax 9-20558 Conformal Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9-20558 Conformal CoatingThick barrier coating; excellent protection of sensitive circuits from moisture. Cure Speed (fpm): 2 - 5 Cure Type: UV/Visible and Heat
Physical Properties Metric English Comments
Viscosity 17000 cP
17000 cP
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 6.89 MPa
1000 psi
Descriptive Properties Value Comments
Cure Depth 0.25 in.