Dymax 6-20481 Fast Shallow Potting Compound and Sealant

Category Polymer , Adhesive , Thermoset
Manufacturer Dymax Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dymax 6-20481 Fast Shallow Potting Compound and Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Shallow Potting and Sealing in SecondsFeaturesUV cures in seconds to 1/4 inch deepOne component, no mixingSolvent-freeEnvironmentally friendlyExcellent adhesion to most substratesDescriptionUV curable potting materials are used for sealing electrical connectors, temperature probes and sensors in applications throughout the aerospace, electronic, electrical, industrial, defense and marine industries. Dymax pitting compounds cure in seconds, on demand, and have very low shrinkage. See pages for a selection of Dymax UV curing lamps and conveyors which can lower production costs when used in conjunction with Dymax adhesives.Dymax 6-20481 Fast Shallow Potting Compound and SealantFlexible, general purpose potting material Key Substrates: Rynite (polyester), Glass, Metal Typical Use: Potting relay screws
Copyright © lookpolymers.com All Rights Reserved