DuPont Teijin Films Teijin® Tetoron® SLA Polyester Film, 200 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Teijin® Tetoron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Teijin® Tetoron® SLA Polyester Film, 200 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Teijin® Tetoron® SLA is a super low shrinkage version of Teijin® Tetoron® type S polyester film. In addition to having the well balanced physical, chemical and electrical properties of type S film, Teijin® Tetoron® SLA has achieved one of the lowest thermal shrinkage characteristics with superior flatness. Teijin® Tetoron® SLA has a lower shrinkage than Teijin® Tetoron® SL. It has a slightly hazy appearance.Typical Applications: Teijin® Tetoron® SLA is suitable for use in many electrical applications where super low thermal shrinkage and superior flatness are very critical, but low haze is not required. Teijin® Tetoron® SLA is recommended for Flexible Printed Circuits (FPC) and Membrane Touch Switches (MTS).Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 160 %
160 %
ASTM D882A
Film Elongation at Break, TD 120 %
120 %
ASTM D882A
Coefficient of Friction, Dynamic 0.36
0.36
ASTM D1894
Coefficient of Friction, Static 0.33
0.33
ASTM D1894
Film Tensile Strength at Break, MD 200 MPa
29000 psi
ASTM D882A
Film Tensile Strength at Break, TD 221 MPa
32000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD <= 0.10 %

@Temperature 150 °C,
Time 1800 sec
<= 0.10 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.00 %

@Temperature 150 °C,
Time 1800 sec
0.00 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM D1003