Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Mylar® ADS Polyester Film, 300 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Mylar®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Mylar® ADS Polyester Film, 300 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mylar® ADS is a heat stabilized, low shrinkage film with good web handling properties. Approvals: UL 94 VTM-2 - for 92 - 500 gauge (0.023 - 0.13mm)Also available in 285 GaugeInformation provided by DuPont.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 95.8 MPa

@Strain >=5.00 %
13900 psi

@Strain >=5.00 %
ASTM D882A
Secant Modulus, MD 3.39 GPa
492 ksi
ASTM D882A
Secant Modulus, TD 4.21 GPa
610 ksi
ASTM D882A
Film Tensile Strength at Break, MD 191 MPa
27700 psi
ASTM D882A
Film Tensile Strength at Break, TD 225 MPa
32600 psi
ASTM D882A
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Shrinkage, MD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 190 °C,
Time 300 sec
1.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Refractive Index 1.64 - 1.67
1.64 - 1.67
typical of Mylar®
Haze 36 %
36 %
ASTM D1003
Transmission, Visible 90.2 %
90.2 %
ASTM D1003
Users viewing this material also viewed the following: