Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Mylar® 840 Polyester Film, 48 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Mylar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Mylar® 840 Polyester Film, 48 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mylar® 840 is a one-side pretreated polyester film for improved metal or cold seal adhesion. The packaging industry is constantly setting higher standards for product protection using flexible packaging films. Improved barriers as well as package strength and stiffness are key characteristics of Mylar® 840 polyester which has made it a premier packaging film.Approvals: FDA Food Contact Status - All gauges of Mylar® 840 comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers, sections (f) and (h). These regulations describe films that can safely be used in contact with all types of foods, excluding alcoholic beverages. The films listed above can be used to contain foods during oven cooking at temperatures up to and above 250°F.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 110 %
110 %
ASTM D882A
Film Elongation at Break, TD 80 %
80 %
ASTM D882A
Coefficient of Friction, Dynamic 0.40
0.40
A-B; ASTM D1894
Coefficient of Friction, Static 0.50
0.50
ASTM D1894
Film Tensile Strength at Break, MD 222 MPa
32200 psi
ASTM D882A
Film Tensile Strength at Break, TD 269 MPa
39000 psi
ASTM D882A
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Maximum Service Temperature, Air 121 °C
250 °F
Shrinkage, MD 1.26 %

@Temperature 150 °C,
Time 1800 sec
1.26 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 1.28 %

@Temperature 150 °C,
Time 1800 sec
1.28 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Refractive Index 1.64 - 1.67
1.64 - 1.67
typical of Mylar®
Transmission, Visible 88.5 %
88.5 %
TLT; ASTM D1003
Descriptive Properties Value Comments
Bond Strength @ Ambient Conditions (metallized) 750 g
77°F and 50% RH
Gas Permeability (Base film) 1.6 cc/100 in2
Nitrogen; ASTM D1434 (24 hrs @ 77°F and 75% RH @ 1 ATM)
31.0 cc/100 in2
Carbon Dioxide; ASTM D1434 (24 hrs @ 77°F and 75% RH @ 1 ATM)
Yield (nominal) 42200 in2/lb
Copyright © lookpolymers.com All Rights Reserved