DuPont Teijin Films Melinex® WLB Polyester Film, 500 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® WLB Polyester Film, 500 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® WLB is a polyester film with a white surface, a light grey surface and very high opacity. General Product Info: Melinex® WLB offers a film with a white surface and very high opacity. It can be coated or extruded with adhesive to be used as an opaque laminate backing. It can also be coated with print receptive coating to directly print an image with no show-through.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 82.7 MPa
12000 psi
ASTM D882A
Film Tensile Strength at Yield, TD 82.7 MPa
12000 psi
ASTM D882A
Film Elongation at Break, MD 120 %
120 %
ASTM D882A
Film Elongation at Break, TD 90 %
90 %
ASTM D882A
Film Tensile Strength at Break, MD 152 MPa
22000 psi
ASTM D882A
Film Tensile Strength at Break, TD 172 MPa
25000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Optical Density >= 4.2
>= 4.2
ASTM D1003
Descriptive Properties Value Comments
Whiteness >100%
ASTM E 313-79