DuPont Teijin Films Melinex® WCW Polyester Film, 92 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® WCW Polyester Film, 92 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® WCW is a translucent white polyester film with a rough surface for superior handling characteristics.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 96.5 MPa
14000 psi
ASTM D882A
Film Tensile Strength at Yield, TD 96.5 MPa
14000 psi
ASTM D882A
Film Elongation at Break, MD 90 %
90 %
ASTM D882A
Film Elongation at Break, TD 60 %
60 %
ASTM D882A
Coefficient of Friction, Dynamic 0.30
0.30
A-B; ASTM D1894
Film Tensile Strength at Break, MD 172 MPa
25000 psi
ASTM D882A
Film Tensile Strength at Break, TD 214 MPa
31000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.8 %

@Temperature 190 °C,
Time 300 sec
2.8 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 0.00 %

@Temperature 190 °C,
Time 300 sec
0.00 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze 82 %
82 %
ASTM D1003
Gloss 18 %
18 %
45°; ASTM D1003
20 %
20 %
60°; ASTM D1003
Transmission, Visible 73 %
73 %
TLT; ASTM D1003
Descriptive Properties Value Comments
Yield (nominal) 21800 in2/lb