DuPont Teijin Films Melinex® RFL1 Polyester Film, 600 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® RFL1 Polyester Film, 600 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MELINEX® RFL1 is a highly reflective, white polyester film. Typical Applications: Typical applications include reflectors in display boards, internally illuminated billboards, labels, backlights, and luminaries. Approvals: UL Recognition - Product has been registered with Underwriters LaboratoriesInformation provided by DuPont.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 80 %
80 %
ASTM D882A
Film Elongation at Break, TD 65 %
65 %
ASTM D882A
Film Tensile Strength at Break, MD 79.3 MPa
11500 psi
ASTM D882A
Film Tensile Strength at Break, TD 86.2 MPa
12500 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 1.7 %

@Temperature 150 °C,
Time 1800 sec
1.7 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 1.2 %

@Temperature 150 °C,
Time 1800 sec
1.2 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Optical Density 1.3
1.3
Densitometer with visual/ortho filter
Gloss 60 %
60 %
60°, Macbeth TD904 Optical; ASTM D2457-08
Transmission, Visible 2.5 %
2.5 %
TLT; ASTM D1003-11
Descriptive Properties Value Comments
Whiteness 110
ASTM E313-79